MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Westlake Plastics Ardel® Polyarylate
Categories: Polymer; Thermoplastic; Polyarylate

Material Notes: Ardel™ PAR polyarylate is a transparent, light-amber colored polymer that exhibits good toughness, superior optical and mechanical properties, exceptional UV stability, and excellent flexural fatigue resistance. Ardel™ PAR is specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement resulting in the formation of a protective layer that essentially serves as a UV stabilizer. Ardel™ PAR is recommended for semiconductor components, solar energy components, appliance parts, and snap lock connectors.

Industry: Engineering; Semiconductor and ESD

Colors Available: Natural

Attributes: Heat Resistant; Dielectric Properties

Shapes: Extruded Slab; Extruded Film; Extruded Sheet

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

New suppliers have been added for this product during the past 60 days.  

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Moisture Absorption 0.260 %0.260 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 69.0 MPa10000 psiASTM D638
Elongation at Break 60 %60 %ASTM D638
Flexural Strength 84.0 MPa
@Strain 5.0 %
12200 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 2.10 GPa304 ksiASTM D790
Izod Impact, Notched 2.25 J/cm4.22 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.02e+7 ohm-cm1.02e+7 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °FASTM D648
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unitika AX-1500 Conditioned
Unitika U-100 Engineering Plastic
Unitika C300VN
NEU Neuthane N8511-1H Aromatic, Polyester TPU Blend
Unitika UG-100-20 Engineering Plastic

PWEST120 / 72752

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.