MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Overview of materials for Zinc Alloy
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Zinc Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by alloying elements or processing methods.

Applications: corrosion protection (galvanization), architectural, automotive, batteries, toys.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 5.02 - 7.17 g/cc0.181 - 0.259 lb/in³Average value: 6.61 g/cc Grade Count:65
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 42.0 - 11942.0 - 119Average value: 72.1 Grade Count:48
Hardness, Knoop 80.0 - 14980.0 - 149Average value: 104 Grade Count:34
Hardness, Rockwell A 36.0 - 46.536.0 - 46.5Average value: 39.6 Grade Count:14
Hardness, Rockwell B 49.0 - 74.049.0 - 74.0Average value: 56.2 Grade Count:20
Hardness, Vickers 30.0 - 13530.0 - 135Average value: 87.3 Grade Count:38
Tensile Strength, Ultimate 37.0 - 441 MPa5370 - 64000 psiAverage value: 259 MPa Grade Count:58
Tensile Strength, Yield 125 - 386 MPa18100 - 56000 psiAverage value: 277 MPa Grade Count:20
Elongation at Break 1.00 - 65.0 %1.00 - 65.0 %Average value: 25.9 % Grade Count:54
Modulus of Elasticity 63.5 - 97.0 GPa9210 - 14100 ksiAverage value: 83.2 GPa Grade Count:14
Compressive Yield Strength 210 - 641 MPa30500 - 93000 psiAverage value: 359 MPa Grade Count:12
Fatigue Strength 28.0 - 172 MPa4060 - 24900 psiAverage value: 60.1 MPa Grade Count:28
Fracture Toughness 12.3 - 23.7 MPa-m½11.2 - 21.6 ksi-in½Average value: 16.3 MPa-m½ Grade Count:6
Shear Strength 138 - 325 MPa20000 - 47100 psiAverage value: 225 MPa Grade Count:18
Charpy Impact, Unnotched 1.40 - 65.0 J1.03 - 47.9 ft-lbAverage value: 34.5 J Grade Count:17
Coefficient of Friction 0.0300 - 0.07000.0300 - 0.0700Average value: 0.0500 Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000580 - 0.00000840 ohm-cm0.00000580 - 0.00000840 ohm-cmAverage value: 0.00000621 ohm-cm Grade Count:56
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.4 - 39.9 µm/m-°C10.8 - 22.2 µin/in-°FAverage value: 26.8 µm/m-°C Grade Count:56
Specific Heat Capacity 0.390 - 0.525 J/g-°C0.0932 - 0.125 BTU/lb-°FAverage value: 0.416 J/g-°C Grade Count:49
Thermal Conductivity 105 - 125 W/m-K727 - 868 BTU-in/hr-ft²-°FAverage value: 109 W/m-K Grade Count:50
Melting Point 375 - 800 °C707 - 1470 °FAverage value: 424 °C Grade Count:60
Solidus 375 - 441 °C707 - 826 °FAverage value: 404 °C Grade Count:54
Liquidus 382 - 502 °C720 - 936 °FAverage value: 424 °C Grade Count:54
 
Processing PropertiesMetricEnglishComments
Processing Temperature 393 - 538 °C740 - 1000 °FAverage value: 456 °C Grade Count:3
Annealing Temperature 105 - 250 °C221 - 482 °FAverage value: 197 °C Grade Count:14
Hot-Working Temperature 120 - 300 °C248 - 572 °FAverage value: 225 °C Grade Count:37
Casting Temperature 395 - 545 °C743 - 1010 °FAverage value: 460 °C Grade Count:16
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.00100 - 50.0 %0.00100 - 50.0 %Average value: 7.48 % Grade Count:70
Cadmium, Cd 0.00200 - 0.450 %0.00200 - 0.450 %Average value: 0.0252 % Grade Count:63
Copper, Cu 0.00100 - 6.00 %0.00100 - 6.00 %Average value: 1.01 % Grade Count:62
Iron, Fe 0.00200 - 0.100 %0.00200 - 0.100 %Average value: 0.0429 % Grade Count:63
Lead, Pb 0.00200 - 1.40 %0.00200 - 1.40 %Average value: 0.0658 % Grade Count:63
Magnesium, Mg 0.00500 - 0.100 %0.00500 - 0.100 %Average value: 0.0236 % Grade Count:31
Tin, Sn 0.00100 - 0.00500 %0.00100 - 0.00500 %Average value: 0.00178 % Grade Count:61
Titanium, Ti 0.120 - 0.500 %0.120 - 0.500 %Average value: 0.294 % Grade Count:7
Zinc, Zn 50.0 - 100 %50.0 - 100 %Average value: 91.7 % Grade Count:73

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc, Zn
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Sand Cast
Overview of materials for Solder/Braze Alloy
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Permanent Mold Cast

M01075 / 81680

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.