System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Arkema Solarkote® H300 Acrylic
Categories:
Polymer
;
Thermoplastic
;
Acrylic (PMMA)
;
Acrylic, UV Stabilized, Molded
Material Notes:
Superior UV protection, Adhesion to HIPS, ASTM Classification PMMA 0233V3
Information provided by Arkema Group
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.15
g/cc
1.15
g/cc
ASTM D792
Water Absorption
0.40 %
0.40 %
24 hr. immersion; ASTM D570
Linear Mold Shrinkage
0.0030
-
0.0080
cm/cm
0.0030
-
0.0080
in/in
ASTM D955
Melt Flow
5.0
g/10 min
@Load 3.80 kg,
Temperature 230 °C
5.0
g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
20
20
ASTM D785
Tensile Strength, Ultimate
32.4
MPa
4700
psi
ASTM D638
Tensile Modulus
1.79
GPa
260
ksi
ASTM D638
Flexural Strength
<=
55.2
MPa
<=
8000
psi
ASTM D790
Flexural Modulus
1.72
GPa
250
ksi
ASTM D790
Izod Impact, Notched
0.481
J/cm
0.900
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Thermal Conductivity
0.216
W/m-K
1.50
BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi)
85.0
°C
185
°F
annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
73.9
°C
165
°F
annealed; ASTM D648
Vicat Softening Point
76.7
°C
170
°F
50°C/hr; 50N; ASTM D1525
91.1
°C
196
°F
50°C/hr; 10N; ASTM D1525
Optical Properties
Metric
English
Comments
Refractive Index
1.49
@Temperature 22.8 °C
1.49
@Temperature 73.0 °F
N
D
; ASTM D542
Haze
<= 2.0 %
@Thickness 3.17 mm
<= 2.0 %
@Thickness 0.125 in
ASTM D1003
Transmission, Visible
89 %
@Thickness 3.17 mm
89 %
@Thickness 0.125 in
ASTM D1003
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Arkema Solarkote® PB Acrylic
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin
Arkema Solarkote® P-600 Acrylic
Arkema Solarkote® P-610 Acrylic
Asahi Kasei DELPET™ SR8200 Acrylic (PMMA), High Impact
PARKG677 / 24398
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.