MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Idemitsu Kosan Xarec® WA 214LG SPS, 40% Glass Filled
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS); Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber

Material Notes: Crystalline Polymer, Glass Filled

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³
Filler Content 40 %40 %
Moisture Absorption 0.010 %0.010 %24 hrs., 50% RH
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 145 MPa21000 psi
Elongation at Break 1.5 %1.5 %
Tensile Modulus 13.7 GPa1990 ksi
Flexural Yield Strength 220 MPa31900 psi
Flexural Modulus 13.2 GPa1910 ksi
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²
Izod Impact, Unnotched (ISO) 40.0 kJ/m²19.0 ft-lb/in²
Charpy Impact Unnotched 4.20 J/cm²20.0 ft-lb/in²
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cm
Dielectric Constant 3.13.1
Dielectric Strength 26.0 kV/mm660 kV/inASTM D145
Dissipation Factor 0.00100.0010IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
8.33 µin/in-°F
@Temperature -22.0 - 86.0 °F
CTE, linear, Transverse to Flow 38.0 µm/m-°C21.1 µin/in-°F
Deflection Temperature at 0.46 MPa (66 psi) 270 °C518 °F
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °F
Flammability, UL94 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 310 °C536 - 590 °F
Mold Temperature 50.0 - 80.0 °C122 - 176 °F
 130 - 155 °C266 - 311 °FFor optimal surface finish
 
Descriptive Properties
Commentslow outgassing @ elevated temperatures
 No mold release

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Idemitsu Kosan Xarec® WA 214 SPS, 40% Glass Filled
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled
Idemitsu Kosan Xarec® EA 522 SPS, 22% Glass Filled
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled

PIDEM111 / 48084

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.