MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Petrothene NA204090 Low Density Polyethylene (LDPE), Wire/Cable Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: Petrothene NA204090 is a natural low density polyethylene resin selected for use as primary insulation for coaxial and control cable applications. NA204090 has also been used as a base resin for compounding materials including gas-injected or chemically expanded insulation. Petrothene NA204090 meets the requirements of ASTM D 1248, Type I, Class A, Category 3, Grade E3. Applications: Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050
Tensile Strength at Break 11.0 MPa1600 psi
Tensile Strength, Yield 10.4 MPa1510 psi
Elongation at Break 550 %550 %
Flexural Modulus, 1% Secant 207 MPa30000 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.28
@Frequency 1e+6 Hz
2.28
@Frequency 1e+6 Hz
Dissipation Factor 0.000060
@Frequency 1e+6 Hz
0.000060
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -76.0 °C<= -105 °F
 
Descriptive Properties
Processing MethodWire & Cable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQT8853 / 220487

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.