MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Lupolen 1800H Low Density Polyethylene (LDPE), Blow Molding Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Lupolen 1800 H is a low density polyethylene resin used in a wide range of processing methods such as injection molding, blow molding and film extrusion. It exhibits very good softness and toughness and good dimensional stability. Lupolen 1800 H is delivered in pellet form and is not additivated. Typical customer applications include caps & closures, lids, foams and champagne corks. Lupolen 1800 H is not intended for use in medical and pharmaceutical applications. Applications: Bottles For Consumer Goods, Caps & Closures, Sports, Leisure & Toys.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ISO 1183-1
Environmental Stress Crack Resistance >= 5.0 hour>= 5.0 hourcond. B, 10% Arkopal N100; ASTM D1693
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545ISO 868
Ball Indentation Hardness 15.0 MPa2180 psiISO 2039-1
Tensile Strength, Yield 9.00 MPa1310 psiISO 527-1,-2
Tensile Modulus 0.200 GPa29.0 ksiISO 527-1,-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 108 °C226 °FISO 3146
Vicat Softening Point 91.0 °C196 °FA50N; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 230 °C356 - 446 °F
 
Descriptive Properties
Ball Indentation Hardness (MPa)H49/30
Processing MethodBlown Film, Extrusion Blow Molding, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 1810 H LDPE, Injection Molding Grade
Chevron Phillips Marlex® 5104 LDPE Blow Molding Resin
LyondellBasell Lupolen 2452 D SW 413 LDPE
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Samyang Tribit® 1800H PBT, Extruding Formality

PEQT8524 / 220159

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.