General purpose, soft type. General CLEAREN (styrene-butadiene block copolymer) information: It has excellent transparency, impact resistance, and hinge performance, and can also be compounded with GPPS without impairing transparency, it is widely used as a reinforcing agent as well. Its molecular structure affords superb transparency, hinge performance, and texture, as well as excellent thermal stability enabling reduced blistering. It also has excellent mold ability, and is a high performance transparent resin that is well-suited to various molding methods including injection and extrusion molding (for forming films and sheets), blow molding, inflation molding, profile extrusion, etc. Uses: Its wide variety of uses include: shrink films, food packaging material sheets, electronic component packaging materials, packaging material sheets for manufacturing, blister packs, ampoules, cosmetic caps, toys, miscellaneous articles, etc. Information provided by Denka Company Limited. |