MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Accuratus Accuflect™ Light-Reflecting Ceramic
Categories: Ceramic; Glaze

Material Notes: Accuflect™ is a specially formulated and processed ceramic developed by Accuratus to satisfy the market demand for diffuse reflectors in high temperature and high energy environments.

Key Property: Highly diffuse reflectance from near UV to Infrared

Typical Uses: Flashlamp pumped solid state laser cavities, Diode laser pumped solid state laser cavities, High temperature diffuse illumination, High temperature lamp housings, Tube furnace radiant energy reflectors

General Information: B6 type Accuflect™ is a porous ceramic usable to 1300 °C. B6 material has enhanced reflectance in the infrared. When the material is used in water cooled cavities or areas of significant contamination a glazed ceramic designated G6 is recommended. G6 is usable to 750 °C.

Accuflect™ reflects 95% to 99% of incident light from 450 nm to 2500 nm. The reflectivity is essentially non-specular with nearly perfect LAMBERTIAN behavior across the entire spectrum.

Accuflect™ is available in two product types. The B6 material has the virgin ceramic surface produced during manufacture. The G6 material has a specialty clear glaze applied to seal the surface porosity of the virgin material, allow easy cleaning and provide a non-contaminating surface where it is exposed to atmosphere or liquid environments.

Information provided by Accuratus.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.30 g/cc0.0831 lb/in³
Porosity 30 %30 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 27.5 MPa3990 psi
Compressive Strength 62.0 MPa8990 psi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.55.5
Dielectric Strength 3.00 kV/mm76.2 kV/in
Dissipation Factor 0.00300.0030
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.70 µm/m-°C4.28 µin/in-°F
Thermal Conductivity 5.80 W/m-K40.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1200 °C2190 °Fno load
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Luminex™ 880 Magnesia
Overview of materials for Silicone, Molded, Glass Fiber Filled
China-Yixing Longly Refractories ASM-120 Cordierite-Mullite
ArcelorMittal AS60 Aluminized steel
Anderman Ceramics EZM 96 Zirconia, 96.5%, Magnesia-Stabilized

CACCUR01 / 129644

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.