MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plenco 7500 Phenolic, Granular, Transfer Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Woodflour Filled

Material Notes: PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component file E40654. 07500 is available in black or red color.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.520 g/cc0.0188 lb/in³ASTM D1895
Density 1.37 g/cc0.0495 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0069 cm/cm0.0069 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 9090ASTM D785
Tensile Strength, Ultimate 52.0 MPa7540 psiASTM D638
Elongation at Break 0.78 %0.78 %ASTM D638
Tensile Modulus 7.70 GPa1120 ksiASTM D638
Flexural Strength 81.0 MPa11700 psiASTM D790
Flexural Modulus 7.40 GPa1070 ksiASTM D790
Compressive Strength 218 MPa31600 psiASTM D695
Poissons Ratio 0.360.36ASTM D638
Shear Modulus 2.83 GPa410 ksiCalculated
Izod Impact, Notched 0.204 J/cm0.382 ft-lb/inASTM D256
Charpy Impact, Notched 0.206 J/cm²0.980 ft-lb/in²ASTM D256
Impact 119119J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.90e+11 ohm-cm3.90e+11 ohm-cmASTM D247
Dielectric Constant 4.84.8ASTM D150
Dielectric Strength 11.1 kV/mm282 kV/inShort Time; ASTM D149
Dissipation Factor 0.0510.051ASTM D150
Arc Resistance 128 sec128 secASTM D495
Comparative Tracking Index 150 V150 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 58.0 µm/m-°C
@Temperature 40.0 - 130 °C
32.2 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.360 W/m-K
@Temperature 100 °C
2.50 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 200 °C392 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 166 °C331 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Oxygen Index 24.7 %24.7 %ASTM D2863
Shrinkage 0.253 %0.253 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLEM42 / 50722

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.