MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Escor™ 5110 ExCo Ethylene Acrylic Acid Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Product Description: Escor 5110 is primarily intended for high speed, low coating weight extrusion coating and extrusion lamination. Excellent adhesion to polar substrates, aluminum foil, polyamide films, metalized films, papers, iron steel and glass. Very high bond resistance even for acidic and aggressive food products. Very low sealing and hot tack initiation temperature, very high hot tack peak force.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Aluminum Containing Packaging
  • Coextrusion Coating
  • Extrusion Coating
  • Extrusion Lamination
  • Food packaging
  • Metalized Films

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.939 g/cc0.0339 lb/in³ExxonMobil method
Acrylic Acid Content 11 %11 %ExxonMobil Method
Melt Flow 14 g/10 min14 g/10 minASTM D1238
Neck In  6.86 cm
@Temperature 280 °C
2.70 in
@Temperature 536 °F
328 ft/min, constant output at 35 rpm; ExxonMobil Method
 14.2 cm
@Temperature 280 °C
5.60 in
@Temperature 536 °F
164 ft/min, constant output at 35 rpm; ExxonMobil Method
Drawdown 6.33 m/s1250 ft/minConstant output at 35 rpm; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 93.9 °C<= 201 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 71.1 °C160 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Escor™ 5200 Ethylene Acrylic Acid Copolymer Resin
ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin
ExxonMobil Escor™ 5020 ExCo Ethylene Acrylic Acid Copolymer Resin
ExxonMobil Escor™ 5100 ExCo Ethylene Acrylic Acid Copolymer Resin
ExxonMobil Escor™ 5050 ExCo Ethylene Acrylic Acid Copolymer Resin

PEX99133 / 175369

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.