MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin  (discontinued **)
Categories: Polymer; Thermoplastic; SMA Polymer; Glass Reinforced, Modified SMA

Material Notes: Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foam

Applications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior trim

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccISO 1183
Filler Content 15 %15 %Glass Fiber; ISO 3451-1
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inISO 2577
Melt Flow 1.1 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.1 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 64.0 MPa9280 psiISO 527-2
Elongation at Yield 2.0 %2.0 %ISO 527-2
Tensile Modulus 4.80 GPa696 ksiISO 527-2
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 4.30 GPa624 ksiISO 178
Izod Impact, Notched (ISO)  4.60 kJ/m²
@Temperature -40.0 °C
2.19 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 2.91 J/cm²13.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.15 J/cm²5.47 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.4 µm/m-°C28.0 µin/in-°FNOVA Chemicals Laboratory Procedure
Deflection Temperature at 1.8 MPa (264 psi) 118 °C
@Thickness 4.00 mm
244 °F
@Thickness 0.157 in
Unannealed; ISO 75-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 227 - 271 °C440 - 520 °FProfile temperatures
Melt Temperature 232 - 271 °C450 - 520 °FAir purge at equilibrium conditions
Mold Temperature 32.2 - 51.7 °C90.0 - 125 °FCore mold surface temperature at equilibrium conditions
 46.1 - 60.0 °C115 - 140 °FCavity mold surface temperature at equilibrium conditions
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Screw Speed 80 - 125 rpm80 - 125 rpm
 
Descriptive Properties
Injection Speedmedium-fast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin
NOVA Chemicals Dylark® 480P12 High Performance Glass Filled Styrenic
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin

PNOV854 / 108462

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.