MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Bynel® 4003 Anhydride-Modified HDPE Adhesive Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene; High Density (HDPE)

Material Notes: Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.

Applications: Bynel® Series 4000 resins are excellent moisture barriers and have a good hydrocarbon resistance. This unique combination of properties makes them useful in a variety of coextrusion applications. HDPE/EVOH tubing and HDPE/polyamide bottles for agricultural chemicals are two examples. Bynel® Series 4000 resins adhere to a variety of materials. They are most often used in coextrusion with EVA, EVOH, polyamide, and PE. Bynel® 4003 is suitable for blown film with polyamide. Bynel® 4006 is appropriate for coextrusion blow molding with either polyamide or EVOH. Bynel® 40E529 can be used for extrusion coating onto paper or bonding to metal surfaces. It provides strong bonds to nylon and good bonds to EVOH in blown film, cast film, and pipe extrusion processes.

Physical properties of Bynel® Series 4000 resins are typical of high-density polyethylene resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others to a particular extrusion process.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ASTM D792
Moisture Vapor Transmission 5.40 cc-mm/m²-24hr-atm13.7 cc-mil/100 in²-24hr-atmASTM E96
Viscosity 2.00e+6 cP
@Shear Rate 50 1/s,
Temperature 190 °C
2.00e+6 cP
@Shear Rate 50 1/s,
Temperature 374 °F
estimated from log-log graph
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 115 °C239 °FFreezing point via DSC/ASTM D3418
 136 °C277 °FMelting point via DSC/ASTM D3418
Vicat Softening Point 129 °C264 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 235 °C455 °FExtruder forward zone and adapter for film or coating with EVA or EVOH
Nozzle Temperature 235 °C455 °FDie

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Radici Radilon® N66-AFR Nylon 66
PTS PPE/Nylon Alloy 10% Glass Filled
Mitsubishi Chemical Advanced Materials Altron™ PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet)
DuPont™ Selar® PA 3426R Nylon Barrier Resin
DuPont Bynel® 4006 Anhydride-Modified HDPE Adhesive Resin

PDUPBQ / 33571

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.