MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Old Hickory No. 6 Kentucky Ball Clay  (discontinued **)
Categories: Ceramic; Clay; Ball Clay

Material Notes: No. 6DC is a highly kaolin clay that can be used as a filler grade material where presence of some 200 M quartz residue is not harmful. Applications can include a variety of refractory compositions as well as non-ceramic building products such as cement and fiberglass reinforced construction board.

Information provided by Old Hickory Clay Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.50 µm0.50 µm50% of particles less than
 0.53 µm0.53 µmMedian particle diameter
 1.0 µm1.0 µm61% of particles less than
 <= 5.0 µm<= 5.0 µm84% of particles less than
pH 6.06.0
Soluble Sulfates 50.0 ppm50.0 ppm
Specific Surface Area 18.8 m²/g18.8 m²/g
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00307 GPa0.445 ksiDry Modulus of Rupture, 50% clay/50% flint, cast bars
 
Thermal PropertiesMetricEnglishComments
Shrinkage 4.6 %4.6 %Cone 04, Linear Fired Shrinkage
 5.5 %5.5 %Linear Drying Shrinkage
 6.0 %6.0 %Cone 3, Linear Fired Shrinkage
 8.0 %8.0 %Cone 11, Linear Fired Shrinkage
 
Component Elements PropertiesMetricEnglishComments
Al2O3 29.05 %29.05 %
CaO 0.12 %0.12 %
Fe2O3 0.99 %0.99 %
K2O 0.52 %0.52 %
Loss on Ignition(%) 9.39 %9.39 %
MgO 0.25 %0.25 %
Na2O 0.080 %0.080 %
SiO2 57.07 %57.07 %
TiO2 2.43 %2.43 %
 
Descriptive Properties
Absorption (%)12.5Cone 3, Fired
 15.2Cone 04, Fired
 6.3Cone 11, Fired
CEC/MBI (meg/100 ml)7.5
Crude ColorWhite
Filtration (ml)25
Pyrometric Cone Equivalent (PCE)32
Water of Plasticity (%)30
Wet Sieve Residue (%)1.05Wet Sieve Residue, +200 mesh

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Old Hickory 44-B Kentucky Ball Clay

EOHC909 / 161988

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.