MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese VECTRA® E530i 30% Mineral Reinforced Liquid Crystal Polymer (LCP)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: Description: Very easy flowing grade with very good heat resistance, good mechanical properties, platable and good impact strength. 30% mineral reinforced.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³ISO 1183
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 4343ISO 2039-2
Tensile Strength at Break 150 MPa21800 psi5 mm/min; ISO 527-2/1A
Elongation at Break 3.5 %3.5 %5 mm/min; ISO 527-2/1A
Tensile Modulus 11.5 GPa1670 ksi1 mm/min; ISO 527-2/1A
Flexural Strength 165 MPa23900 psiISO 178
Flexural Modulus 11.7 GPa1700 ksiISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 22.0 kJ/m²10.5 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 8.40 J/cm²40.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 2.90 J/cm²13.8 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 44.0 kV/mm1120 kV/inIEC 60243-1
Dissipation Factor 0.0257
@Frequency 1e+6 Hz
0.0257
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 V225 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.00 µm/m-°C
@Temperature 20.0 °C
1.11 µin/in-°F
@Temperature 68.0 °F
ISO 11359-2
CTE, linear, Transverse to Flow 34.0 µm/m-°C
@Temperature 20.0 °C
18.9 µin/in-°F
@Temperature 68.0 °F
ISO 11359-2
Melting Point 335 °C635 °FISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FISO 75-1, -2
Flammability, UL94 V-0V-0thickness h
Oxygen Index 40 %40 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 315 - 325 °C599 - 617 °F
Middle Barrel Temperature 325 - 335 °C617 - 635 °F
Front Barrel Temperature 330 - 340 °C626 - 644 °F
Nozzle Temperature 335 - 345 °C635 - 653 °F
Melt Temperature 335 - 345 °C635 - 653 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Vectra® C130 Liquid Crystal Polymer (LCP), 30% Glass Reinforced
Celanese VECTRA S475 LCP, 32% Mineral / Glass Reinforced
Celanese VECTRA® C810 Glass/Mineral Filled Liquid Crystal Polymer (LCP)
Celanese VECTRA E830iPd LCP, 30% Specialty
Celanese VECTRA E820iPd LCP, 42% Specialty

PHCW78 / 46019

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.