MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Epoxy, Cast, Unreinforced
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.490 - 1.80 g/cc0.0177 - 0.0649 lb/in³Average value: 1.19 g/cc Grade Count:34
Water Absorption 0.100 - 3.90 %0.100 - 3.90 %Average value: 0.474 % Grade Count:20
Viscosity 200 - 180000 cP200 - 180000 cPAverage value: 17100 cP Grade Count:48
 46.0 - 1500 cP
@Temperature 65.0 - 100 °C
46.0 - 1500 cP
@Temperature 149 - 212 °F
Average value: 632 cP Grade Count:8
Linear Mold Shrinkage 0.00100 - 0.00700 cm/cm0.00100 - 0.00700 in/inAverage value: 0.00189 cm/cm Grade Count:9
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 87.0 - 93.087.0 - 93.0Average value: 91.0 Grade Count:6
Hardness, Rockwell M 85.0 - 12185.0 - 121Average value: 100 Grade Count:6
Hardness, Shore D 6.00 - 90.06.00 - 90.0Average value: 65.1 Grade Count:40
 >= 70.0
@Temperature 120 - 120 °C
>= 70.0
@Temperature 248 - 248 °F
Average value: 70.0 Grade Count:6
Tensile Strength, Ultimate 7.58 - 179 MPa1100 - 26000 psiAverage value: 51.9 MPa Grade Count:54
Elongation at Break 0.420 - 140 %0.420 - 140 %Average value: 14.6 % Grade Count:45
Modulus of Elasticity 0.827 - 10.4 GPa120 - 1500 ksiAverage value: 5.63 GPa Grade Count:16
Flexural Yield Strength 13.8 - 207 MPa2000 - 30000 psiAverage value: 79.6 MPa Grade Count:36
Flexural Modulus 0.0138 - 5.34 GPa2.00 - 775 ksiAverage value: 3.15 GPa Grade Count:16
Compressive Yield Strength 13.8 - 279 MPa2000 - 40500 psiAverage value: 108 MPa Grade Count:37
Compressive Modulus 0.629 - 3.34 GPa91.3 - 485 ksiAverage value: 1.22 GPa Grade Count:7
Izod Impact, Notched 0.246 - 1.13 J/cm0.460 - 2.12 ft-lb/inAverage value: 0.430 J/cm Grade Count:9
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 9.00e+16 ohm-cm1.00e+12 - 9.00e+16 ohm-cmAverage value: 7.25e+15 ohm-cm Grade Count:32
 1.00e+8 - 1.00e+15 ohm-cm
@Temperature 66.0 - 130 °C
1.00e+8 - 1.00e+15 ohm-cm
@Temperature 151 - 266 °F
Average value: 7.80e+13 ohm-cm Grade Count:7
Surface Resistance 5.42e+11 - 7.85e+15 ohm5.42e+11 - 7.85e+15 ohmAverage value: 2.41e+15 ohm Grade Count:11
Dielectric Constant 2.80 - 5.302.80 - 5.30Average value: 3.87 Grade Count:28
 2.66 - 5.60
@Temperature 100 - 150 °C
2.66 - 5.60
@Temperature 212 - 302 °F
Average value: 4.06 Grade Count:12
 2.66 - 5.60
@Frequency 60.0 - 1000 Hz
2.66 - 5.60
@Frequency 60.0 - 1000 Hz
Average value: 4.06 Grade Count:12
Dielectric Strength 11.8 - 21.7 kV/mm300 - 550 kV/inAverage value: 16.0 kV/mm Grade Count:23
Dissipation Factor 0.00500 - 0.05500.00500 - 0.0550Average value: 0.0218 Grade Count:18
 0.00700 - 0.142
@Temperature 100 - 150 °C
0.00700 - 0.142
@Temperature 212 - 302 °F
Average value: 0.0580 Grade Count:11
 0.00700 - 0.142
@Frequency 60.0 - 60.0 Hz
0.00700 - 0.142
@Frequency 60.0 - 60.0 Hz
Average value: 0.0580 Grade Count:11
Arc Resistance 150 sec150 secAverage value: 150 sec Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 33.0 - 65.0 µm/m-°C18.3 - 36.1 µin/in-°FAverage value: 39.8 µm/m-°C Grade Count:7
Thermal Conductivity 0.167 - 0.795 W/m-K1.16 - 5.52 BTU-in/hr-ft²-°FAverage value: 0.468 W/m-K Grade Count:19
Maximum Service Temperature, Air 45.0 - 300 °C113 - 572 °FAverage value: 115 °C Grade Count:52
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90.0 %90.0 %Average value: 90.0 % Grade Count:11
 
Processing PropertiesMetricEnglishComments
Cure Time 40.0 - 30200 min0.667 - 504 hourAverage value: 2260 min Grade Count:17
 20.0 - 3600 min
@Temperature 50.0 - 180 °C
0.333 - 60.0 hour
@Temperature 122 - 356 °F
Average value: 204 min Grade Count:33
Pot Life 15.0 - 4320 min15.0 - 4320 minAverage value: 349 min Grade Count:63
 16.0 - 420 min
@Temperature 60.0 - 100 °C
16.0 - 420 min
@Temperature 140 - 212 °F
Average value: 93.8 min Grade Count:20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Cure Resin
Overview of materials for Epoxy Adhesive
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Overview of materials for Epoxy/Carbon Fiber Composite
Overview of materials for Epoxy Molding Compound

O1700 / 77888

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.