MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Film

Material Notes: TF-0438-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability. It is also biologically and chemically inert.

The NOVA Chemicals Material Safety Data Sheet contains important safety information and should be reviewed before using the product.

Features: Excellent stiffness and gloss

Additives: High temperature AO

Applications: Blending, Co-extruded films

Film properties are Typical of cast film extruded at 280°C.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³ASTM D 792
Thickness 20.0 microns0.787 mil
Melt Flow 4.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 15.0 MPa2180 psiASTM D 882
Film Tensile Strength at Yield, TD 15.0 MPa2180 psiASTM D 882
Film Elongation at Break, MD 600 %600 %ASTM D 882
Film Elongation at Break, TD 900 %900 %ASTM D 882
Elmendorf Tear Strength MD 19 g19 gASTM D 1922
Elmendorf Tear Strength TD 320 g320 gASTM D 1922
Elmendorf Tear Strength, MD 0.950 g/micron24.1 g/milASTM D 1922
Elmendorf Tear Strength, TD 16.0 g/micron406 g/milASTM D 1922
Film Tensile Strength at Break, MD 38.0 MPa5510 psiASTM D 882
Film Tensile Strength at Break, TD 26.0 MPa3770 psiASTM D 882
1% Secant Modulus, MD 340 MPa49300 psiASTM D 882
1% Secant Modulus, TD 430 MPa62400 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %3.0 %ASTM D 1003
Gloss 88 %88 %45°; ASTM D 2457
 
Descriptive Properties
Low Friction Puncture3 (ft-lb/mil)NOVA Chemicals test method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin

PNOV816 / 108876

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.