MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

GRECO ISOPAK® 735 SAN
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Characteristics: High Flow General Injection

Application: Daily Commodities

Information provided by Great Eastern Resins Industrial Co. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Melt Flow 24 g/10 min
@Load 10.0 kg,
Temperature 220 °C
24 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8383ASTM D785
Tensile Strength at Break 68.6 MPa
@Thickness 0.0625 mm
9950 psi
@Thickness 0.00246 in
5 mm/min; ASTM D638
Tensile Strength, Yield 69.6 MPa
@Thickness 0.0625 mm
10100 psi
@Thickness 0.00246 in
5 mm/min; ASTM D638
Flexural Yield Strength 108 MPa15600 psi2.8mm/min; ASTM D790
Flexural Modulus 3.33 GPa483 ksi2.8mm/min; ASTM D790
Izod Impact, Notched 0.196 J/cm0.367 ft-lb/in1/8" x 1/2" x 5/2"; ASTM D256 Method A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
@Diameter 12.7 mm
196 °F
@Diameter 0.500 in
ASTM D648
Vicat Softening Point 104 °C
@Load 1.00 kg
219 °F
@Load 2.20 lb
ASTM D1525
Flammability, UL94 HBHBFile no. E85466

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRECO5239 / 282222

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.