MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sika Level-325 High Strength, cementitious, self leveling underlayment for interior and exterior
Categories: Ceramic; Concrete

Material Notes: Sika® Level-325 is a one-component, durable and versatile cementitious underlayment for interior and exterior concrete and cementitious substrates. It can be applied manually or by pump to produce a self-smoothing, rapid-setting and flat substrate prior to the application of a final floor finish. Typical application thickness is 1/8” up to 1.5” (3 up to 38 mm), or up to 3” (76 mm) with aggregate.

Where to Use:

  • Concrete
  • Cement substrates
  • Rapid drying cement screed systems
  • OSB/Plywood only suitable for flexible coverings
  • Old substrates such as ceramic tiles and terrazzo
  • Old, water-resistant adhesive residues
Advantages:
  • Self-leveling
  • For interior and exterior use
  • High strength
  • Low shrinkage
  • Manual or pumpable application
  • Zero VOC content and low odor
  • Levels new and old floors
  • Can accept caster wheel loading if the thickness is greater than 1/8’’
  • No MVER (Moisture Vapor Emission Rate) limits on well prepared concrete

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.13 g/cc0.0770 lb/in³
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/lEPA method 24
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 10.3 MPa
@Time 2.42e+6 sec
1500 psi
@Time 672 hour
ASTM C348
Compressive Strength  13.8 MPa
@Time 86400 sec
2000 psi
@Time 24.0 hour
ASTM C109
 24.1 MPa
@Time 605000 sec
3500 psi
@Time 168 hour
ASTM C109
 36.5 MPa
@Time 2.42e+6 sec
5300 psi
@Time 672 hour
ASTM C109
 
Processing PropertiesMetricEnglishComments
Cure Time 70.0 - 90.0 min1.17 - 1.50 hourInitial set; ASTM C191
 80.0 - 110 min1.33 - 1.83 hourFinal set; ASTM C191
 240 min4.00 hourReady for Foot Traffic
 240 min4.00 hourReady for Tiles or Stone
 1440 min24.0 hourReady for Floor Covering
Working Life 30.0 min30.0 min
Shelf Life 12.0 Month
@Temperature 5.00 - 30.0 °C
12.0 Month
@Temperature 41.0 - 86.0 °F
in original unopened cartridge
 
Descriptive Properties
ColorConcrete gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Concrete, Lightweight
Autoclaved aerated concrete, 0.750 g/cc density
Concrete; Stone, 1-2-4 Mix
Autoclaved aerated concrete, 0.800 g/cc density
Concrete, 1-4 Dry

PSIKA910 / 209817

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.