System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Sumitomo Bakelite North America RX® 1-501N Mineral Filled Diallyl Phthalate
Categories:
Polymer
;
Thermoset
;
Diallyl Phthalate (DAP)
;
Diallyl Phthalate (DAP), Cast, Mineral Filler
;
Filled/Reinforced Thermoset
Material Notes:
Mineral filled diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG.
Information provided by Vyncolit, a Sumitomo Bakelite Group
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.80
g/cc
0.0650
lb/in³
Relative Density; ASTM D792
Linear Mold Shrinkage
0.0030
-
0.0060
cm/cm
0.0030
-
0.0060
in/in
Compression Molding; ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
55.2
MPa
8010
psi
ASTM D638
Flexural Strength
110
MPa
16000
psi
At Rupture; ASTM D790
Flexural Modulus
11.7
GPa
1700
ksi
ASTM D790
Compressive Strength
145
MPa
21000
psi
ASTM D695
Izod Impact, Notched
0.240
J/cm
0.450
ft-lb/in
ASTM D256
Electrical Properties
Metric
English
Comments
Dielectric Constant
3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
Wet; ASTM D150
4.2
@Frequency 1000 Hz
4.2
@Frequency 1000 Hz
wet; ASTM D150
Dielectric Strength
15.8
kV/mm
401
kV/in
60Hz, Step-by-Step, wet; ASTM D149
Dissipation Factor
0.013
@Frequency 1000 Hz
0.013
@Frequency 1000 Hz
wet; ASTM D150
0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance
140
sec
140
sec
ASTM D495
Comparative Tracking Index
>=
600
V
>=
600
V
IEC 112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
25.0
µm/m-°C
@Temperature 20.0 °C
13.9
µin/in-°F
@Temperature 68.0 °F
ASTM E-831
Maximum Service Temperature, Air
130
°C
266
°F
UL 746B
Deflection Temperature at 1.8 MPa (264 psi)
166
°C
331
°F
As molded; ASTM D648
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Descriptive Properties
Color
Black, Blue, Brown, Green, Red
Form
Granular
Main Filler
Mineral
Molding Method
Compression, transfer, injection
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac
Sumitomo Bakelite North America RX® 3-2-530-P Long-Glass Reinforced Diallyl Phthalate
Sumitomo Bakelite RX® 1310 Diallyl Ortho-Phthalate Molding Compound
PVYNC056 / 72264
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.