MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mocom (ALBIS) ALCOM® PA66 910/1.1 CF40 Nylon 66, 40% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Carbon Fiber Filled

Material Notes: Base Polymer: Polyamide 66

Filler/Additive System: 40% Carbon fibers

Special Features: Electrically conductive, reduced surface resistivity, heat ageing stabilization, high stiffness

Market Segment: Automotive, Machinery

Application Area: Injection molded parts

Typical Applications: Functional components

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Time 86400 sec
0.0010 - 0.0030 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0030 - 0.0040 cm/cm
@Time 86400 sec
0.0030 - 0.0040 in/in
@Time 24.0 hour
ISO 294-4
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 245 MPa35500 psiISO 527
Elongation at Break 2.0 %2.0 %ISO 527
Tensile Modulus 27.0 GPa3920 ksiISO 527
Flexural Strength 360 MPa52200 psiISO 178
Flexural Modulus 23.0 GPa3340 ksiISO 178
Charpy Impact Unnotched 5.50 J/cm²26.2 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10 ohm-cm10 ohm-cmIEC 62631-3-1
Surface Resistance <= 10 ohm<= 10 ohmIEC 62631-3-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FISO 75-1/-2
Vicat Softening Point 255 °C491 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection molding
Mold Temperature 80.0 - 120 °C176 - 248 °FInjection molding
Drying Temperature <= 80.0 °C
@Time 7200 - 43200 sec
<= 176 °F
@Time 2.00 - 12.0 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyamide 66

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® C3 GF 40 1 (4658) PA66/6 Dry, 40% Glass Filled
Akro-Plastic Akromid® C3 GF 40 1 (4658) PA66/6 Conditioned, 40% Glass Filled
Premix Thermoplastics PRESEAL 6070 Ag-Coated Glass
Premix Thermoplastics PRE-ELEC® PP 1380
LNP Lexan® SML5897 Polycarbonate, 40% Carbon Fiber Reinforced

PALBIS8111 / 242170

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.