MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Toyobo GLAMIDE® T-714E Transparent Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon, Aromatic

Material Notes: GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing and a specific grade approved as UL94V-0 class is provided, and it exhibits excellent chemical resistance and oil resistance. Grade T-714E is a non-reinforced, non-spherulite, aromatic, and transparent nylon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccAbsolute Drying; ASTM-D792
Water Absorption 1.3 %1.3 %Absolute Drying; ASTM-D570
Moisture Absorption at Equilibrium 2.4 %2.4 %Absolute Drying; ASTM-D570
Linear Mold Shrinkage  0.0010 - 0.0030 cm/cm
@Thickness 1.00 mm
0.0010 - 0.0030 in/in
@Thickness 0.0394 in
Absolute Drying
 0.0040 - 0.0070 cm/cm
@Thickness 3.00 mm
0.0040 - 0.0070 in/in
@Thickness 0.118 in
Absolute Drying
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120Absolute Drying; ASTM-D785
Tensile Strength, Ultimate  16.0 MPa
@Temperature 80.0 °C
2320 psi
@Temperature 176 °F
Practical Use (Water Absorption 2.4%); ASTM-D638
 80.0 MPa
@Temperature 80.0 °C
11600 psi
@Temperature 176 °F
Absolute Drying; ASTM-D638
 92.0 MPa
@Temperature 23.0 °C
13300 psi
@Temperature 73.4 °F
Practical Use (Water Absorption 2.4%); ASTM-D638
 97.0 MPa
@Temperature 23.0 °C
14100 psi
@Temperature 73.4 °F
Absolute Drying; ASTM-D638
 125 MPa
@Temperature -40.0 °C
18100 psi
@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D638
 130 MPa
@Temperature -40.0 °C
18900 psi
@Temperature -40.0 °F
Absolute Drying; ASTM-D638
Elongation at Break 50 %50 %ASTM-D638
Flexural Strength  25.0 MPa
@Temperature 80.0 °C
3630 psi
@Temperature 176 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
 121 MPa
@Temperature 80.0 °C
17500 psi
@Temperature 176 °F
Absolute Drying; ASTM-D790
 135 MPa
@Temperature 23.0 °C
19600 psi
@Temperature 73.4 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
 147 MPa
@Temperature 23.0 °C
21300 psi
@Temperature 73.4 °F
Absolute Drying; ASTM-D790
 185 MPa
@Temperature -40.0 °C
26800 psi
@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
 195 MPa
@Temperature -40.0 °C
28300 psi
@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Flexural Modulus  0.500 GPa
@Temperature 80.0 °C
72.5 ksi
@Temperature 176 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
 2.00 GPa
@Temperature 80.0 °C
290 ksi
@Temperature 176 °F
Absolute Drying; ASTM-D790
 2.50 GPa
@Temperature 23.0 °C
363 ksi
@Temperature 73.4 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
 2.60 GPa
@Temperature 23.0 °C
377 ksi
@Temperature 73.4 °F
Absolute Drying; ASTM-D790
 3.50 GPa
@Temperature -40.0 °C
508 ksi
@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
 3.80 GPa
@Temperature -40.0 °C
551 ksi
@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Compressive Strength 100 MPa14500 psiAbsolute Drying; ASTM-D695
Izod Impact, Notched  0.200 J/cm
@Temperature -40.0 °C
0.375 ft-lb/in
@Temperature -40.0 °F
ASTM-D256
 0.600 J/cm
@Temperature 23.0 °C
1.12 ft-lb/in
@Temperature 73.4 °F
ASTM-D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM-D257
Dielectric Constant 4.0
@Frequency 1000 Hz
4.0
@Frequency 1000 Hz
ASTM-D150
Dielectric Strength 19.0 kV/mm
@Thickness 2.00 mm
483 kV/in
@Thickness 0.0787 in
ASTM-D149
Arc Resistance 110 sec110 secASTM-D495
Comparative Tracking Index >= 600 V>= 600 VIEC Method
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 µm/m-°C30.0 µin/in-°FAbsolute Drying; ASTM-D696
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FAbsolute Drying; ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °FAbsolute Drying; ASTM-D648
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °F
Mold Temperature 60.0 °C140 °F
Injection Pressure 40.0 - 50.0 MPa5800 - 7250 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 30 nat PA*
EMS-Grivory Grilamid® TR 30 LS nat PA*
EMS-Grivory Grilamid® TR 55 PA12/MACMI
EMS-Grivory Grilamid® TR 55 LY PA12/MACMI
EMS-Grivory Grilamid® TR 55 LX PA12/MACMI

PTOY917 / 107468

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.