MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Vinnolit® SA 1062/7 Vinyl Chloride/Vinyl Acetate Copolymer Extender resin
Categories: Polymer; Thermoplastic; Vinyl (PVC); Polyvinyl Chloride - Polyvinyl Acetate Copolymer

Material Notes: Vinnolit® SA 1062/7 Vinyl chloride/vinyl acetate copolymer extender resin for paste application. Vinnolit® 1062/7 is a copolymeric extender resin which has been specially developed for paste making. In blends with paste making PVC resins, it combines the good viscosity-reducing properties of the homopolymer paste extender resins with the lower gelling temperatures typical of vinyl acetate copolymers. By incorporating an extender resin such as Vinnolit® SA 1062/7 processing can be improved as the viscosity is considerable reduced, particularly in low plasticizer content and highly filled plastisols. By exchanging part of a copolymer paste resin the storage stability, dilatancy and deaeratibility are improved. In addition, the vinyl acetate content enables to lower gelling temperatures. Adhesion to various substrates, such as metal and synthetic fibers is improved. Vinnolit® SA 1062/7 is suited for automotive underbody sealants, carpet backing and laminating pastes. Vinnolit® SA 1062/7 can be processed by all the standard methods, such as coating, dipping, casting and spraying. Vinnolit® SA 1062/7 is especially used in automotive underbody coatings and sealants.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %ISO 1269
Apparent Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Particle Size <= 100 µm<= 100 µm<= 0.5% Retained on 0.1 mm Sieve; DIN EN ISO 53195
Viscosity Test 92 cm³/g0.92 dl/gReduced Viscosity; ISO 1628-2
Vinyl Acetate Content 7.0 %7.0 %
 
Descriptive Properties
K-Value61ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVINNO921 / 291118

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.