MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

V-36 Cobalt Alloy
Categories: Metal; Superalloy; Cobalt Base

Material Notes: High-temperature sheets

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.70 g/cc0.314 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  34.5 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
5000 psi
@Temperature 1800 °F,
Time 1000 hour
 58.6 MPa
@Temperature 982 °C,
Time 360000 sec
8500 psi
@Temperature 1800 °F,
Time 100 hour
 124 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
18000 psi
@Temperature 1500 °F,
Time 1000 hour
 159 MPa
@Temperature 816 °C,
Time 360000 sec
23000 psi
@Temperature 1500 °F,
Time 100 hour
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.1 µm/m-°C
@Temperature 20.0 - 100 °C
6.72 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 12.6 W/m-K
@Temperature 20.0 - 100 °C
87.0 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.27 %0.27 %
Chromium, Cr 25 %25 %
Cobalt, Co 46.33 %46.33 %Balance
Iron, Fe 3.0 %3.0 %
Manganese, Mn 1.0 %1.0 %
Nickel, Ni 20 %20 %
Niobium, Nb (Columbium, Cb) 2.0 %2.0 %
Silicon, Si 0.40 %0.40 %
Tungsten, W 2.0 %2.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MTEK N155 UNS R30155 Severe Corrosion and Heat Resistant Alloy
Weartech International WT-12 Cobalt Hardfacing & Wear Resistant Alloy
Less Common Metals SmCo5 Samarium Cobalt Alloy; Vacuum Induction Melting & Casting
Latrobe MP35N® Alloy
Kennametal Stellite Stellite® F Cobalt Alloy

NZ97084 / 191476

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.