MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Geon® Performance Solutions Vinyl Packaging M2211 PVC, Rigid  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, High Impact; PVC, Rigid Grade

Material Notes: Medical USP VI in Transparent 9445 color only

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D792
Apparent Bulk Density 0.801 g/cc0.0289 lb/in³ASTM D1505
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8181ASTM D2240
Tensile Strength, Yield 49.0 MPa7110 psiType I, 51 mm/min; ASTM D638
Tensile Modulus 2.62 GPa380 ksiType I, 51 mm/min; ASTM D638
Flexural Strength 84.8 MPa12300 psiASTM D790
Flexural Modulus 2.79 GPa405 ksiASTM D790
Izod Impact, Notched 7.15 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
13.4 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 66.1 °C
@Thickness 6.35 mm
151 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 210 °C390 - 410 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood Contact, Unspecified Rating
USP Class VI YesYes
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesFood Contact Acceptable
 High Gloss
 High Impact Resistance
FormsPellets
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesBottles
 Packaging
 Sheet

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH1PN8714 / 102550

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.