MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Gharda Chemicals Gafone S 1320GF Polysulfone (PS)  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes:

Characteristics:

  • High Temperature Resistance - Tg 189°C
  • Excellent Clarity
  • Excellent Mechanical & Electrical properties
  • Easy to process
  • Very good Hydrolytic Resistance

Applications:

  • Electrical & Electronic - Head lamp reflectors, Chip tray carriers, battery cases
  • Industrial - Milking machine parts, Safety belts
  • Medical - Surgical tools, Dialysis membranes
  • Membrane applications

Information provided by Gharda Chemicals

Solvay Advanced Polymers completed its acquisition of this product line in May 2006.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Filler Content 20 %20 %
Water Absorption 0.50 %0.50 %24 Hours; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Tensile Modulus 6.50 GPa943 ksiASTM D638
Flexural Strength 148 MPa21500 psiASTM D790
Flexural Modulus 6.50 GPa943 ksiASTM D790
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
Dielectric Constant 2.8
@Frequency 60 Hz
2.8
@Frequency 60 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm559 kV/inASTM D149
Dissipation Factor 0.0030
@Frequency 60 Hz
0.0030
@Frequency 60 Hz
ASTM D150
Arc Resistance 60 sec60 secASTM D495
Comparative Tracking Index 150 V150 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 165 °C329 °FContinuous Use; UL-746B
Deflection Temperature at 1.8 MPa (264 psi) 183 °C361 °FASTM D648
Glass Transition Temp, Tg 187 °C369 °FASTM D3482
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
Oxygen Index 35 %35 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGHARDA42 / 41815

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.