MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Avient Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Information provided by PolyOne™ Corporation

Key Words: Multi-Purpose
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/ccASTM D792
Water Absorption 0.25 %
@Thickness 3.17 mm
0.25 %
@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 257 MPa37300 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 1.0 - 3.0 %1.0 - 3.0 %Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 17.2 GPa2500 ksiType 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 310 MPa45000 psiASTM D790
Flexural Modulus 13.8 GPa2000 ksiASTM D790
Izod Impact, Notched 1.33 J/cm2.50 ft-lb/inMethod A, Injection Molded, 0.125 in bars, 73°F; ASTM D648
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 302 °C575 °FUnannealed, 0.125 in bars; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 321 - 349 °C610 - 660 °FMolding
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced
DuPont Mobility and Materials Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA)
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced
MTI ThermoStran® PPA-50G Long Glass Fiber Compound
RTP Company RTP 4009 MS 2  Polyphthalamide (PPA) Glass Fiber 50% - Molybdenum Disulfide 2%

PH1PO3472 / 45096

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.