MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Goodfellow Aluminum EN AC 42100
Categories: Metal; Intermetallic

Material Notes:

Information provided by Goodfellow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.675 g/cc0.09664 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 6060
Tensile Strength 175 MPa25400 psi
Elongation at Break 8 %8 %
Modulus of Elasticity 74.0 GPa10700 ksi
Shear Strength 621 MPa90000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000400 ohm-cm0.00000400 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.5 µm/m-°C
@Temperature 20.0 - 100 °C
11.9 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 160 W/m-K
@Temperature 20.0 - 100 °C
1110 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
Melting Point 555 °C1030 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.7 %91.7 %
Magnesium, Mg 0.3 %0.3 %
Silicon, Si 7 %7 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Molybdenum Disilicide, MoSi2
Alnico® 4 (Isotropic, Cast) Hard Magnetic Alloy
Cobalt Samarium 1 Hard Magnetic Alloy
Goodfellow Nd2Fe14B Neodymium Iron Boron Magnetic Material
Magnesium Silicide, Mg2Si

NGOODF114x / 197416

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.