MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lotte Advanced Materials Starex® CT-0510 Transparent Grade ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
Melt Flow 20 g/10 min
@Load 10.0 kg,
Temperature 220 °C
20 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength, Yield 44.1 MPa
@Thickness 3.17 mm
6400 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 50 %
@Thickness 3.17 mm
50 %
@Thickness 0.125 in
ASTM D638
Flexural Strength 66.9 MPa
@Thickness 3.17 mm
9700 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.14 GPa
@Thickness 3.17 mm
310 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched  0.961 J/cm
@Thickness 6.35 mm
1.80 ft-lb/in
@Thickness 0.250 in
ASTM D256
 1.17 J/cm
@Thickness 3.17 mm
2.20 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 6.35 mm
176 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point 93.0 °C199 °FUnannealed; ISO R 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %
@Thickness 3.00 mm
90 %
@Thickness 0.118 in
plate, NP
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °FInjection Temp
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 75.0 - 80.0 °C167 - 176 °F
Dry Time 2 - 4 hour2 - 4 hour
Injection Pressure 68.5 - 107.7 MPa9940 - 15620 psi
Back Pressure 0.979 - 1.96 MPa142 - 284 psi
Screw Speed 60 - 90 rpm60 - 90 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-758 ABS - Transparent
Chi Mei Polylac® PA-758R ABS - Transparent
Ineos ABS Lustran® 266 ABS, Transparent Grade
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness
Aclo Accucomp ABS ABS881L Clear Grade

PLBST000 / 50482

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.