MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Mitsubishi Chemical Advanced Materials Cestilene™ HD 500 Polyethylene  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ISO 1183
Water Absorption 0.010 %0.010 %immersion
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464after 15 sec.; ISO 868
 6666after 3 sec.; ISO 868
Ball Indentation Hardness 45.0 MPa6530 psiISO 2039-1
Tensile Strength, Yield 28.0 MPa4060 psiISO 527
Elongation at Break >= 50 %>= 50 %ISO 527
Elongation at Yield 10 %10 %ISO 527
Tensile Modulus 1.35 GPa196 ksiISO 527
Compressive Yield Strength 9.00 MPa1310 psiat 1% nominal strain; ISO 604
 15.0 MPa2180 psiat 2% nominal strain; ISO 604
 23.0 MPa3340 psiat 5% nominal strain; ISO 604
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 10.5 J/cm²50.0 ft-lb/in²Partial Break; ISO 179/1eA
Abrasion 350350Relative loss per DSM internal test (CESTILENE HD 1000 = 100)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmIEC 93
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 93
Dielectric Constant  2.4
@Frequency 100 Hz
2.4
@Frequency 100 Hz
IEC 250
 2.4
@Frequency 1e+6 Hz
2.4
@Frequency 1e+6 Hz
IEC 250
Dielectric Strength <= 45.0 kV/mm<= 1140 kV/inIEC 243
Dissipation Factor  0.00020
@Frequency 100 Hz
0.00020
@Frequency 100 Hz
IEC 250
 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 600 V600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 175 - 225 µm/m-°C
@Temperature 20.0 °C
97.2 - 125 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
Melting Point 130 - 135 °C266 - 275 °FISO 3146; DSC, 10°C/min
Maximum Service Temperature, Air 80.0 °C176 °F20,000 hours continuous
 120 °C248 °Ffor short periods
Deflection Temperature at 1.8 MPa (264 psi) 44.0 °C111 °FISO 75 method A
Vicat Softening Point 80.0 °C176 °FISO 306
Minimum Service Temperature, Air -100 °C-148 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Oxygen Index <= 20 %<= 20 %ISO 4589
 
Descriptive Properties
Colornatural (white)/black

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Bamberger Polymers Bapolene® 3252 Polyethylene, Injection Grade
Network Polymers NPP 50-0151
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
Network Polymers NPP 50-0350

P1SN00 / 20187

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.