MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³
Linear Mold Shrinkage, Flow 0.0040 - 0.0065 cm/cm0.0040 - 0.0065 in/in
Linear Mold Shrinkage, Transverse 0.0080 - 0.011 cm/cm0.0080 - 0.011 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  30.0 MPa
@Temperature 150 °C
4350 psi
@Temperature 302 °F
 40.0 MPa
@Temperature 120 °C
5800 psi
@Temperature 248 °F
 50.0 MPa
@Temperature 90.0 °C
7250 psi
@Temperature 194 °F
 65.0 MPa
@Temperature 60.0 °C
9430 psi
@Temperature 140 °F
 95.0 MPa
@Temperature 23.0 °C
13800 psi
@Temperature 73.4 °F
Elongation at Break  1.7 %
@Temperature 23.0 °C
1.7 %
@Temperature 73.4 °F
 2.0 %
@Temperature 60.0 °C
2.0 %
@Temperature 140 °F
 2.4 %
@Temperature 90.0 °C
2.4 %
@Temperature 194 °F
 2.8 %
@Temperature 120 °C
2.8 %
@Temperature 248 °F
 3.0 %
@Temperature 150 °C
3.0 %
@Temperature 302 °F
Tensile Modulus  2.70 GPa
@Temperature 150 °C
392 ksi
@Temperature 302 °F
 3.50 GPa
@Temperature 120 °C
508 ksi
@Temperature 248 °F
 5.00 GPa
@Temperature 90.0 °C
725 ksi
@Temperature 194 °F
 7.80 GPa
@Temperature 60.0 °C
1130 ksi
@Temperature 140 °F
 11.0 GPa
@Temperature 23.0 °C
1600 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 475 V475 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °F
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °F
Vicat Softening Point 205 °C
@Load 5.00 kg
401 °F
@Load 11.0 lb
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
Oxygen Index 30 %30 %
Glow Wire Test  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 255 °C464 - 491 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 110 - 130 °C
@Time 10800 sec
230 - 266 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC 605 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 5209 Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC 610 Mineral Filled, Glass Reinforced Polyester Compound
A. Schulman BMC 5307 Mineral Filled, Glass Reinforced Polyester
LATI LATER 4 G/20-V0 20% Glass Fiber Reinforced Polybutylene terephthalate (PBT) (UL94 V-0)

PLATH9785 / 177481

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.