Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Pocan® A 3121 901510 PBT+ASA, 20% Glass Fiber
Categories:
Polymer
;
Thermoplastic
;
ASA Polymer
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
PBT + ASA Blend, Glass Fiber Reinforced
Material Notes:
PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finish
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.43
g/cc
1.43
g/cc
ISO 1183
Bulk Density
0.700
g/cc
0.0253
lb/in³
ISO 60
Moisture Absorption at Equilibrium
0.10 %
0.10 %
50% RH; ISO 62
Water Absorption at Saturation
0.40 %
0.40 %
ISO 62
Linear Mold Shrinkage, Flow
0.0010
cm/cm
0.0010
in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
0.0030
cm/cm
0.0030
in/in
60x60x2; 270°C / MT 90°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0020
cm/cm
0.0020
in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
0.0070
cm/cm
0.0070
in/in
60x60x2; 270°C / MT 90°C; 600 bar; ISO 294-4
Melt Flow
20
g/10 min
@Load 2.16 kg,
Temperature 270 °C
20
g/10 min
@Load 4.76 lb,
Temperature 518 °F
ISO 1133-1
Mechanical Properties
Metric
English
Comments
Ball Indentation Hardness
157
MPa
22800
psi
ISO 2039-1
Tensile Strength at Break
110
MPa
16000
psi
ISO 527-1, -2; 5 mm/min
Elongation at Break
2.9 %
2.9 %
ISO 527-1, -2; 5 mm/min
Tensile Modulus
7.00
GPa
1020
ksi
ISO 527-1, -2; 1 mm/min
Flexural Strength
170
MPa
@Strain 3.2 %
24700
psi
@Strain 3.2 %
2 mm/min; ISO 178-A
Flexural Modulus
7.00
GPa
1020
ksi
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
<=
4.76
ft-lb/in²
ISO 180-1A
Izod Impact, Unnotched (ISO)
45.0
kJ/m²
@Temperature -30.0 °C
21.4
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
50.0
kJ/m²
@Temperature 23.0 °C
23.8
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched
4.00
J/cm²
@Temperature -30.0 °C
19.0
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
5.50
J/cm²
@Temperature 23.0 °C
26.2
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Puncture Energy
2.20
J
1.62
ft-lb
ISO 6603-2
Electrical Properties
Metric
English
Comments
Comparative Tracking Index
200
V
200
V
d.a.m.; Solution A; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
30.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
16.7
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1, -2
CTE, linear, Transverse to Flow
90.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Melting Point
225
-
260
°C
437
-
500
°F
10°C/min; ISO 11357-1, -3
Deflection Temperature at 0.46 MPa (66 psi)
215
°C
419
°F
ISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi)
175
°C
347
°F
ISO 75-1, -2
Vicat Softening Point
165
°C
@Load 5.10 kg
329
°F
@Load 11.2 lb
120°C/hour; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Processing Properties
Metric
English
Comments
Melt Temperature
260
-
280
°C
500
-
536
°F
270
°C
518
°F
for test specimens; ISO 294
Mold Temperature
80.0
-
100
°C
176
-
212
°F
90.0
°C
194
°F
for test specimens; ISO 294
Drying Temperature
120
°C
248
°F
Dry Time
4
-
8
hour
4
-
8
hour
Moisture Content
0.00 - 0.020 %
0.00 - 0.020 %
residual; Karl Fischer Test
Descriptive Properties
Flammability Test
passed
ISO 3795; US-FMVSS302
ISO Short Name
ISO 7792-1-PBT+PET+ASA, GHMR, 07-070, GF20
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Mytex Polymers AS171L-02US Polypropylene, 13% Talc Filled
Techmer ES HiFill® ASA GF15 15% Glass Filled
Lanxess Pocan® TP 740-201 000000 PBT + ASA, 20% Glass Fiber
INEOS Styrolution Luran® S KR2858 G3 Acrylonitrile Styrene Acrylate (ASA)
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled
PLANX0655 / 133618
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.