Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
;
Syndiotactic Polystyrene (SPS)
Material Notes:
Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.38
g/cc
0.0499
lb/in³
Filler Content
30 %
30 %
Moisture Absorption
0.010 %
0.010 %
24 hrs., 50% RH
Linear Mold Shrinkage, Flow
0.0010
-
0.0030
cm/cm
0.0010
-
0.0030
in/in
Linear Mold Shrinkage, Transverse
0.0040
-
0.0070
cm/cm
0.0040
-
0.0070
in/in
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
125
MPa
18100
psi
Elongation at Break
2.0 %
2.0 %
Tensile Modulus
10.7
GPa
1550
ksi
Flexural Yield Strength
195
MPa
28300
psi
Flexural Modulus
10.5
GPa
1520
ksi
Izod Impact, Notched (ISO)
10.0
kJ/m²
4.76
ft-lb/in²
Izod Impact, Unnotched (ISO)
33.0
kJ/m²
15.7
ft-lb/in²
Charpy Impact Unnotched
4.20
J/cm²
20.0
ft-lb/in²
Charpy Impact, Notched
1.20
J/cm²
5.71
ft-lb/in²
Electrical Properties
Metric
English
Comments
Electrical Resistivity
1.00e+16
ohm-cm
1.00e+16
ohm-cm
Dielectric Constant
3.1
3.1
Dielectric Strength
32.0
kV/mm
813
kV/in
ASTM D145
Dissipation Factor
0.0020
0.0020
IEC 60250
Arc Resistance
60
-
120
sec
60
-
120
sec
ASTM D495
Comparative Tracking Index
250
-
400
V
250
-
400
V
IEC 60112
Hot Wire Ignition, HWI
60
-
120
sec
@Thickness 1.50 mm
60
-
120
sec
@Thickness 0.0591 in
UL 746A
High Amp Arc Ignition, HAI
>=
120
arcs
@Thickness 1.50 mm
>=
120
arcs
@Thickness 0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR
0.000
-
10.0
mm/min
0.000
-
0.394
in/min
UL746A
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
19.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
10.6
µin/in-°F
@Temperature -22.0 - 86.0 °F
CTE, linear, Transverse to Flow
39.0
µm/m-°C
21.7
µin/in-°F
Deflection Temperature at 0.46 MPa (66 psi)
265
°C
509
°F
Deflection Temperature at 1.8 MPa (264 psi)
245
°C
473
°F
UL RTI, Electrical
125
°C
257
°F
UL746B
UL RTI, Mechanical with Impact
120
°C
248
°F
UL746B
UL RTI, Mechanical without Impact
120
°C
248
°F
UL746B
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Processing Properties
Metric
English
Comments
Melt Temperature
280
-
310
°C
536
-
590
°F
Mold Temperature
50.0
-
80.0
°C
122
-
176
°F
130
-
155
°C
266
-
311
°F
For optimal surface finish
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled
DuPont Mobility and Materials Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
Idemitsu Kosan Xarec® EA 528 SPS, 30% Glass Filled
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled
PIDEM101c / 48073
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.