MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Arkema OREVAC® 18510 Grafted Maleic Anhydride Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene

Material Notes: OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe coating to have good adhesion performances between an epoxy primer and the HDPE 4206 black or LACQTENE 2006PBK35 from Total Petrochemicals. OREVAC 18510 combined with MD or HDPE and a proper epoxy fulfill the requirement of different application standards such as NFA 49-710 or DIN 30670 when applied in the rules of art.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ISO 1183
Melt Index of Compound 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 608
Tensile Strength, Yield 25.0 MPa3630 psiISO R 527-2
Elongation at Break 600 %600 %ISO R 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 134 °C273 °FDSC
Vicat Softening Point 121 °C
@Load 0.999 kg
250 °F
@Load 2.20 lb
ISO 306
 
Processing PropertiesMetricEnglishComments
Zone 1 160 - 180 °C320 - 356 °F
Zone 2 180 - 200 °C356 - 392 °F
Zone 3 200 - 220 °C392 - 428 °F
Zone 4 210 - 230 °C410 - 446 °F
Die Temperature 220 - 240 °C428 - 464 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema OREVAC® 18350 Grafted Maleic Anhydride Polyethylene
Arkema OREVAC® 18365 Maleic Anhydride Modified Polyethylene
Arkema OREVAC® 18380 Maleic Anhydride Modified Polyethylene
Arkema OREVAC® 18319 Grafted Maleic Anhydride Polyethylene
Arkema OREVAC® 18390 Maleic Anhydride Modified Polyethylene

PARKG131 / 80117

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.