MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

GMR-235D Cast Nickel Superalloy
Categories: Metal; Superalloy; Nickel Base

Material Notes: Typical Applications: Jet engine parts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.05 g/cc0.291 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  121 MPa
@Temperature 982 °C,
Time 360000 sec
17500 psi
@Temperature 1800 °F,
Time 100 hour
 269 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
39000 psi
@Temperature 1500 °F,
Time 1000 hour
 386 MPa
@Temperature 816 °C,
Time 360000 sec
56000 psi
@Temperature 1500 °F,
Time 100 hour
 689 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
100000 psi
@Temperature 1200 °F,
Time 1000 hour
 758 MPa
@Temperature 649 °C,
Time 360000 sec
110000 psi
@Temperature 1200 °F,
Time 100 hour
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.8 µm/m-°C
@Temperature 20.0 - 100 °C
7.11 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 11.7 W/m-K
@Temperature 20.0 - 100 °C
81.2 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 3.5 %3.5 %
Boron, B 0.050 %0.050 %
Carbon, C 0.15 %0.15 %
Chromium, Cr 15.5 %15.5 %
Manganese, Mn <= 0.10 %<= 0.10 %
Nickel, Ni >= 73.4 %>= 73.4 %As Balance
Silicon, Si <= 0.30 %<= 0.30 %
Titanium, Ti 2.5 %2.5 %
Zirconium, Zr 4.5 %4.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GMR-235 Cast Nickel Superalloy
AISI 1215 Steel, cold drawn, 19-38 mm round

NZ97008 / 191409

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.