MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta ES1 Melamine Paper Laminate Sheet, NEMA ES-1
Categories: Polymer; Thermoset; Melamine

Material Notes: Composed of white melamine paper core with various pigmented cover sheets.

Information provided by Norplex-Micarta

Key Words: Paper, Melamine, Micarta, NEMA ES-1
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc
@Thickness 12.7 mm
1.40 g/cc
@Thickness 0.500 in
ASTM D792
Moisture Absorption 2.50 %
@Thickness 1.57 mm
2.50 %
@Thickness 0.0620 in
ASTM D570 Condition A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100
@Thickness 6.35 mm
100
@Thickness 0.250 in
ASTM D785
Tensile Strength  63.4 MPa
@Thickness 3.17 mm
9200 psi
@Thickness 0.125 in
CrossWise; ASTM D638 Condition A
 72.4 MPa
@Thickness 3.17 mm
10500 psi
@Thickness 0.125 in
LengthWise; ASTM D638 Condition A
Flexural Strength  93.1 MPa
@Thickness 1.57 mm
13500 psi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
 93.1 MPa
@Thickness 1.57 mm
13500 psi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
Flexural Modulus  10.3 GPa
@Thickness 1.57 mm
1500 ksi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
 10.3 GPa
@Thickness 1.57 mm
1500 ksi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
Compressive Strength 172 MPa
@Thickness 12.7 mm
25000 psi
@Thickness 0.500 in
Flatwise; ASTM D695 Condition A
Izod Impact, Unnotched  0.294 J/cm
@Thickness 12.7 mm
0.550 ft-lb/in
@Thickness 0.500 in
CrossWise; ASTM D256 Condition E-48/50
 0.320 J/cm
@Thickness 12.7 mm
0.600 ft-lb/in
@Thickness 0.500 in
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown  5000 V
@Thickness 1.57 mm
5000 V
@Thickness 0.0620 in
ASTM D149 Condition D-48/50
 50000 V
@Thickness 1.57 mm
50000 V
@Thickness 0.0620 in
ASTM D149 Condition A
Arc Resistance 120 sec
@Thickness 3.17 mm
120 sec
@Thickness 0.125 in
ASTM D495 Conition A
 
Thermal PropertiesMetricEnglishComments
UL RTI, Mechanical with Impact 120 °C248 °FUL Bulletin 746b
Flammability, UL94 V-0
@Thickness 1.57 mm
V-0
@Thickness 0.0620 in
 
Descriptive Properties
Bonding Strength1000[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta BR60 Phenolic Canvas Laminate Sheet
Norplex-Micarta MC511FR Epoxy Glass Laminate Sheet, NEMA FR-5
Norplex-Micarta MC511AF Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta MC511A Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta MC507U Silicone Glass Laminate Sheet, NEMA G-7

PNORPM077 / 192834

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.