MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plenco 4504 Phenolic, Granular, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Cellulose Filled

Material Notes: Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical properties, it has found use in a wide variety of wiring device applications. It is UL recognized under file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.660 g/cc0.0238 lb/in³ASTM D1895
Density 1.57 g/cc0.0567 lb/in³ASTM D792
Water Absorption 0.223 %0.223 %ASTM D570
Linear Mold Shrinkage 0.00283 cm/cm0.00283 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 8383ASTM D785
Tensile Strength, Ultimate 49.0 MPa7110 psiASTM D638
Elongation at Break 0.51 %0.51 %ASTM D638
Tensile Modulus 11.3 GPa1640 ksiASTM D638
Flexural Strength 74.0 MPa10700 psiASTM D790
Flexural Modulus 9.80 GPa1420 ksiASTM D790
Compressive Strength 183 MPa26500 psiASTM D695
Izod Impact, Notched 0.174 J/cm0.326 ft-lb/inASTM D256
Charpy Impact, Notched 0.207 J/cm²0.985 ft-lb/in²ASTM D256
Impact 9898J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+12 ohm-cm3.00e+12 ohm-cmASTM D247
Dielectric Constant 5.15.1ASTM D150
Dielectric Strength 13.1 kV/mm333 kV/inShort Time; ASTM D149
Dissipation Factor 0.0440.044ASTM D150
Arc Resistance 171 sec171 secASTM D495
Comparative Tracking Index 200 V200 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 191 °C376 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Shrinkage 0.127 %0.127 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 2308 Phenolic, Granular, Transfer Molded
Plenco 2308 Phenolic, Granular, Injection Molded
Plenco 2369 Phenolic, Granular, Compression Molded
Plenco 2311 Phenolic, Granular, Transfer Molded
Plenco 2311 Phenolic, Granular, Injection Molded

PLEL89m / 50663

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.