MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Titanium Grade 3, Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Information provided by Allvac and the references.

Applications: Airframe skin, heat exchangers, cryogenic vessels, components for CPI equipment, condenser tubing, exhaust pipe shrouds. Sample was annealed 2 hr at 700°C.

Forms typically available: billet, bar, plate, sheet, strip, rod, wire, extrusions, tubing.

Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.

Key Words: ASTM Grade 3; UNS R50550, CP titanium, C.P. titanium alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.50 g/cc0.163 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 225225
Hardness, Knoop 289289Estimated from Rockwell C.
Hardness, Rockwell C 2626
Hardness, Vickers 280280Estimated from Rockwell C.
Tensile Strength 234 MPa
@Temperature 316 °C
33900 psi
@Temperature 601 °F
Tensile Strength, Ultimate 520 MPa75400 psi
Tensile Strength, Yield 450 MPa65300 psi
Elongation at Break 25 %25 %
Creep Strength 103 MPa
@Temperature 316 °C,
Time >=3.60e+6 sec
14900 psi
@Temperature 601 °F,
Time >=1000 hour
strain 3%
Rupture Strength >= 172 MPa
@Temperature 316 °C,
Time 3.60e+6 sec
>= 24900 psi
@Temperature 601 °F,
Time 1000 hour
Tensile Modulus 104 GPa15100 ksi
Modulus of Rigidity 38.6 GPa5600 ksi
Compressive Modulus 114 GPa16500 ksi
Notched Tensile Strength 790 MPa115000 psiKt (stress concentration factor) = 3.0
Ultimate Bearing Strength 920 MPa133000 psi
Bearing Yield Strength 650 MPa94300 psi
Poissons Ratio 0.340.34
Fatigue Strength  250 MPa
@# of Cycles 1.00e+7
36300 psi
@# of Cycles 1.00e+7
Kt (stress concentration factor) = 2.7
 280 MPa
@# of Cycles 1.00e+7
40600 psi
@# of Cycles 1.00e+7
 290 MPa
@# of Cycles 1.00e+6
42100 psi
@# of Cycles 1.00e+6
 295 MPa
@# of Cycles 100000
42800 psi
@# of Cycles 100000
 340 MPa
@# of Cycles 10000
49300 psi
@# of Cycles 10000
 340 MPa
@# of Cycles 1.00e+7
49300 psi
@# of Cycles 1.00e+7
unnotched
Shear Modulus 39.0 GPa5660 ksi
Charpy Impact 27.0 J19.9 ft-lbV-notch
Bend Radius, Minimum 2.5 t
@Thickness >=1.80 mm
2.5 t
@Thickness >=0.0709 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000540 ohm-cm0.0000540 ohm-cm
 0.0000900 ohm-cm
@Temperature 250 °C
0.0000900 ohm-cm
@Temperature 482 °F
 0.000120 ohm-cm
@Temperature 500 °C
0.000120 ohm-cm
@Temperature 932 °F
 0.000150 ohm-cm
@Temperature 750 °C
0.000150 ohm-cm
@Temperature 1380 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 325 J/g140 BTU/lbHigh Purity Ti.
CTE, linear  8.60 µm/m-°C
@Temperature 20.0 - 93.0 °C
4.78 µin/in-°F
@Temperature 68.0 - 199 °F
 9.20 µm/m-°C
@Temperature 200 °C
5.11 µin/in-°F
@Temperature 392 °F
 19.9 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
perpendicular
Specific Heat Capacity 0.523 J/g-°C0.125 BTU/lb-°F
 0.560 J/g-°C
@Temperature 200 °C
0.134 BTU/lb-°F
@Temperature 392 °F
 0.620 J/g-°C
@Temperature 400 °C
0.148 BTU/lb-°F
@Temperature 752 °F
 0.690 J/g-°C
@Temperature 600 °C
0.165 BTU/lb-°F
@Temperature 1110 °F
Thermal Conductivity 16.4 W/m-K114 BTU-in/hr-ft²-°F
 18.1 W/m-K
@Temperature 200 °C
126 BTU-in/hr-ft²-°F
@Temperature 392 °F
 18.1 W/m-K
@Temperature 400 °C
126 BTU-in/hr-ft²-°F
@Temperature 752 °F
 19.1 W/m-K
@Temperature 600 °C
133 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 21.5 W/m-K
@Temperature 800 °C
149 BTU-in/hr-ft²-°F
@Temperature 1470 °F
Melting Point <= 1660 °C<= 3020 °F
Liquidus 1660 °C3020 °F
Beta Transus 920 °C1690 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.30
@Temperature 710 °C
0.30
@Temperature 1310 °F
High purity Ti
Reflection Coefficient, Visible (0-1) 0.560.56High purity Ti; visible light.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.30 %<= 0.30 %
Nitrogen, N <= 0.050 %<= 0.050 %
Other, total <= 0.30 %<= 0.30 %
Oxygen, O <= 0.35 %<= 0.35 %
Titanium, Ti 99.1 %99.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 2, Annealed
Titanium Ti-6Al-4V (Grade 5), Annealed
Aluminum 6061-T6; 6061-T651
ATI Wah Chang Nb/Nb Alloy C-103
304 Stainless Steel (UNS S30400); Annealed Sheet

MTU031 / 14262

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.