MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CeramTec 192/193 Titania
Categories: Ceramic; Oxide; Titanium Oxide

Material Notes: 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gray in color and conducts static electricity.

Key Words: TiO2, Titanium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.00 g/cc0.145 lb/in³DIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %0.00 %DIN EN 623-2 / ASTM-C373
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 800800HV 0.5; DINV ENV 843-4
Tensile Strength at Break 51.6 MPa7480 psiACMA Test #4 / DIN EN 843-1
Tensile Modulus 228 GPa33100 ksiYoung's; DINV ENV 843-2 / ASTM-F417
Flexural Strength 137 MPa19900 psi20 x 40 mm
Compressive Strength 688 MPa99800 psiASTM C-773-88 / DIN 51067T1
Poissons Ratio 0.270.27DINV ENV 843-2
Fracture Toughness 3.20 MPa-m½2.91 ksi-in½DIN 51109
Shear Modulus 89.0 GPa12900 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  10000 ohm-cm
@Temperature 900 °C
10000 ohm-cm
@Temperature 1650 °F
 1.70e+6 ohm-cm
@Temperature 500 °C
1.70e+6 ohm-cm
@Temperature 932 °F
 9.80e+11 ohm-cm
@Temperature 100 °C
9.80e+11 ohm-cm
@Temperature 212 °F
IEC 672-1
 >= 1.00e+12 ohm-cm
@Temperature 25.0 °C
>= 1.00e+12 ohm-cm
@Temperature 77.0 °F
ASTM-D257
Dielectric Constant 85
@Frequency 1e+6 Hz
85
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Strength 3.937 kV/mm100.0 kV/in6.35 mm (1/4") IEC 672-1
Dissipation Factor  0.00050
@Frequency 1e+6 Hz
0.00050
@Frequency 1e+6 Hz
 0.0010
@Frequency 60.0 Hz
0.0010
@Frequency 60.0 Hz
 0.0040
@Frequency 1e+10 Hz
0.0040
@Frequency 1e+10 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.80 µm/m-°C4.89 µin/in-°FDIN EN 821-1
 8.30 µm/m-°C
@Temperature 20.0 - 200 °C
4.61 µin/in-°F
@Temperature 68.0 - 392 °F
 9.00 µm/m-°C
@Temperature 20.0 - 600 °C
5.00 µin/in-°F
@Temperature 68.0 - 1110 °F
ASTM-C373
 9.00 µm/m-°C
@Temperature 20.0 - 1000 °C
5.00 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.700 J/g-°C
@Temperature 100 - 200 °C
0.167 BTU/lb-°F
@Temperature 212 - 392 °F
DINV ENV 821-3
Thermal Conductivity 11.9 W/m-K82.6 BTU-in/hr-ft²-°FDIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 1000 °C1830 °F
 
Descriptive Properties
ColorTan/Gray
Te Value (°C)520
Thermal Shock Resistance R1 (K)330Hasselman (Experimental)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Anderman Ceramics EM60P Sillimanite
Titanium Dioxide, Brookite
Titanium Dioxide, Rutile
Chemours Teflon® PTFE Grade 7B Granular Compression Molding Resin
Overview of materials for Silicone Rubber

CCERA938 / 107538

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.