MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Exxtral™ BNU 013 Performance Polyolefin
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior applications such as door panels.

Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, South America and North America

Features:

  • Balanced Stiffness/Toughness
  • Good Impact Resistance
  • Good Processability
  • High Scratch Resistance
  • High Stiffness
  • Medium Flow
Uses:
  • Automotive Applications
  • Automotive Interior Parts
  • Automotive Interior Trim
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
16 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 13.0 MPa1890 psiISO 527-2
Tensile Strength, Yield 17.0 MPa2470 psiISO 527-2
Elongation at Yield 4.0 %4.0 %ISO 527-2
Tensile Modulus 1.01 GPa146 ksiSecant; ISO 527-2
Flexural Modulus 1.03 GPa149 ksiISO 178
Charpy Impact, Notched  0.903 J/cm²
@Temperature -20.0 °C
4.30 ft-lb/in²
@Temperature -4.00 °F
Complete Break; ISO 179
 1.30 J/cm²
@Temperature 0.000 °C
6.20 ft-lb/in²
@Temperature 32.0 °F
Complete Break; ISO 179
 2.10 J/cm²
@Temperature 22.8 °C
10.0 ft-lb/in²
@Temperature 73.0 °F
Complete Break; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C156 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-2/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exxtral™ BNU 011 Performance Polyolefin
Dow Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Covestro Bayblend® T65 HG PC/ABS Blend
Dow Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer
Dow Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer

PEX99353 / 175589

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.