MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Old Hickory APG-300 Kentucky Ball Clay
Categories: Ceramic; Clay; Ball Clay

Material Notes: This is an extremely low 325 Mesh wet residue clay. It can be employed in a variety of applications where high purity mineral filler is required. It has a moderate GE brightness value and is particularly beneficial where suspension of other materials is important or where low settling tendency is critical.

Information provided by Old Hickory Clay Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.60 g/cc2.60 g/cc
Brightness 69 %69 %GE Brightness
Oil Absorption 40 %40 %
Moisture Absorption <= 2.00 %<= 2.00 %
Particle Size 0.40 µm0.40 µmMedian particle diameter
 0.50 µm0.50 µm57% of particles less than
 1.0 µm1.0 µm68% of particles less than
 2.0 µm2.0 µm77% of particles less than
 5.0 µm5.0 µm90% of particles less than
 10 µm10 µm96% of particles less than
 <= 20 µm<= 20 µm99% of particles less than
pH 6.06.0
 
Component Elements PropertiesMetricEnglishComments
Al2O3 29.2 %29.2 %
CaO 0.090 %0.090 %
Fe2O3 0.81 %0.81 %
K2O 0.12 %0.12 %
Loss on Ignition(%) 9.8 %9.8 %
MgO 0.19 %0.19 %
Na2O 0.54 %0.54 %
SiO2 56.4 %56.4 %
TiO2 2.26 %2.26 %
 
Descriptive Properties
Crude ColorCream, White, Tan
Wet Sieve Residue (%)0.5Wet Sieve Residue, +325 mesh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EOHC904 / 161983

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.