MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

International Mold Steel DC53 General-Purpose Cold Work Die and Mold Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Mold Steel

Material Notes: Description: DC53 is a general-purpose cold work die and mold steel whose strength and toughness approach those of high-speed steels.

Unique Characteristics:

  • Higher hardness (62-63 HRc) than D2 after heat treatment.
  • Twice the toughness of D2 with superior wear resistance.
  • 20% higher fatigue strength than D2.
  • Smaller primary carbides than D2 protect the die from chipping and cracking
  • Secondary refining process (DLF) reduces impurities.
  • Machines and grinds up to 40% faster than D2.
  • Less residual stress after wire EDMing.

Applications:

  • Plastic Molds
  • Stepped punch and press-punching dies
  • Concrete sprayer parts, rotor plates
  • Swaging dies and backers
  • Dies for cold forging
  • Thread-rolling circular dies
  • Piercing punch
  • Thread-rolling dies for heat-treated bolts
  • Forming dies
  • Stripper plates for lead frame blanking
  • Gauges
  • Screws for injection molding machines

Information provided by International Mold Steel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.76 g/cc7.76 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 210 - 225210 - 225Annealed
Hardness, Rockwell C 62 - 6362 - 63
Modulus of Elasticity 150 GPa21700 ksi
Poissons Ratio 0.280.28
Fatigue Strength 833 MPa
@# of Cycles 1.00e+6
121000 psi
@# of Cycles 1.00e+6
Heat treatment: 1030°C, 520°C (x2), HRc63
Shear Modulus 58.5 GPa8480 ksiModulus of Rigidity
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.95 %0.95 %
Chromium, Cr 8.0 %8.0 %
Iron, Fe 87.35 %87.35 %As Balance
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 2.0 %2.0 %
Silicon, Si 1.0 %1.0 %
Vanadium, V 0.30 %0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Misumi DC53 JIS Tool Steel
JIS S45C Steel, Tempered
JIS SKD11 Tool Steel
Latrobe LSS™ D2 Tool Steel (ASTM D2)
Assab Steels STAVAX Supreme Plastic Mold Material

NIMS07 / 17386

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.