MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet
Categories: Polymer; Thermoset; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 2.00 g/cc1.80 - 2.00 g/ccIEC 1212-2 8.1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 250 MPa>= 36300 psiIEC 1212-2 5.7
Flexural Strength >= 400 MPa>= 58000 psiPerpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 22.0 GPa>= 3190 ksiIEC 1212-2 5.2
Compressive Strength >= 400 MPa>= 58000 psiPerpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 35.0 MPa>= 5080 psiParallel to laminations; IEC 1212-2 5.6
Charpy Impact Unnotched >= 7.00 J/cm²>= 33.3 ft-lb/in²Parallel to laminations; IEC 1212-2 5.5.2
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+8 ohm>= 1.00e+8 ohmAfter immersion in water; IEC 1212-2 6.3
Dielectric Constant  <= 5.5
@Frequency 48.0 - 62.0 Hz
<= 5.5
@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
 <= 5.5
@Frequency 1e+6 Hz
<= 5.5
@Frequency 1e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 40000 V
@Temperature 90.0 °C
>= 40000 V
@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor  <= 0.030
@Frequency 48.0 - 62.0 Hz
<= 0.030
@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
 <= 0.030
@Frequency 1e+6 Hz
<= 0.030
@Frequency 1e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 150 V>= 150 VIEC 1212-2 6.4
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HBHBIEC 1212-2 7.2
 
Descriptive Properties
Thermal Endurance160 T.I.IEC 1212-2 7.1
Water Absorption< 127 mgIEC 1212-2 8.2; Test piece 50 x 50 x 10 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1045 Steel, Quenched and Tempered to 390 HB
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
Hippe PI
JIS S45C Steel, Normalized

PHIPPE929 / 121933

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.