MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Molded

Material Notes: Uses include electric/electronic parts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM D792
Water Absorption 0.3 %
@Time 86400 sec
0.3 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow  0.006 - 0.008 cm/cm
@Thickness 3.00 mm
0.006 - 0.008 in/in
@Thickness 0.118 in
ASTM D955
 0.007 - 0.009 cm/cm
@Thickness 2.00 mm
0.007 - 0.009 in/in
@Thickness 0.0787 in
ASTM D955
Linear Mold Shrinkage, Transverse  0.007 - 0.009 cm/cm
@Thickness 3.00 mm
0.007 - 0.009 in/in
@Thickness 0.118 in
ASTM D955
 0.008 - 0.010 cm/cm
@Thickness 2.00 mm
0.008 - 0.010 in/in
@Thickness 0.0787 in
ASTM D955
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 280 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 536 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 71.6 MPa
@Thickness 3.20 mm
10400 psi
@Thickness 0.126 in
ASTM D638
Elongation at Break 20 %
@Thickness 3.17 mm
20 %
@Thickness 0.125 in
ASTM D638
Flexural Strength 117 MPa
@Thickness 3.20 mm
17000 psi
@Thickness 0.126 in
ASTM D790
Flexural Modulus 2.45 GPa
@Thickness 3.20 mm
356 ksi
@Thickness 0.126 in
ASTM D790
Izod Impact, Notched  0.785 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
1.47 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
 0.981 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
1.84 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
 1.96 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
3.67 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
@Thickness 3.20 mm
275 °F
@Thickness 0.126 in
Unannealed; ASTM D648
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0 - 5VA
@Thickness 2.00 mm
V-0 - 5VA
@Thickness 0.0787 in
 V-0 - 5VA
@Thickness 3.00 mm
V-0 - 5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 280 °C482 - 536 °F
Middle Barrel Temperature 260 - 290 °C500 - 554 °F
Front Barrel Temperature 260 - 300 °C500 - 572 °F
Nozzle Temperature 260 - 300 °C500 - 572 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 90 - 100 °C190 - 212 °F
Dry Time 3 - 4 hour3 - 4 hour
Moisture Content >= 0.01 %>= 0.01 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUMILOY GN1006F Injection Molding FR mPPO
Shinil Chemical SHINCON MPPO Electro Conductive Polymer
Aluminum 1060-H16
Beijing Chemical Industry KAIFA® M105N MPPO Resin
Beijing Chemical Industry KAIFA® M105 MPPO Resin

PLGCHEM258 / 146091

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.