MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Gromax Melamine (Fine Grade)
Categories: Polymer; Thermoset; Melamine

Material Notes: China K

Information provided by Gromax Enterprises Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 10 - 32 Mesh10 - 32 Mesh0%
 32 - 60 Mesh32 - 60 Mesh0%
 60 - 100 Mesh60 - 100 Mesh0.21%
 100 - 200 Mesh100 - 200 Mesh0.26%
 200 - 325 Mesh200 - 325 Mesh1.88%
 >= 325 Mesh>= 325 Mesh97.65%
pH 7.5 - 9.57.5 - 9.5
Maximum Moisture Content 0.100.10
Ash <= 0.030 %<= 0.030 %
 
Descriptive Properties
Ammelide0.0002Typical
Ammeline0.001Typical
AppearanceWhite crystalline powder
Color<20APHA
 <20APHA
Gravity Ratio0.38Typical
Purity>99.8%
Turbidity<20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Melamine-Phenolic Copolymer
Pyrotek TS-105 Thermoset Electrical Insulation Product (Nema Grade: G-5)
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System
Overview of materials for Thermoset Polyurethane, Liquid
Overview of materials for Thermoset Fluoroelastomer

PGROM002 / 147815

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.