lib.mat{1}.name='Titanium Ti-6Al-2Sn-4Zr-2Mo-0.1Si; Duplex Annealed'; lib.mat{1}.variables.alpha='0.0000077'; lib.mat{1}.variables.rho='4540'; lib.mat{1}.variables.sigma='526315.8'; lib.mat{1}.variables.C='460'; lib.mat{1}.variables.nu='0.325'; lib.mat{1}.variables.mu='5.1E+10'; lib.mat{1}.variables.Sys='1.05E+09'; lib.mat{1}.variables.k='7'; lib.mat{2}.name='Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si)'; lib.mat{2}.variables.alpha='0.000009'; lib.mat{2}.variables.rho='4500'; lib.mat{2}.variables.sigma='625000'; lib.mat{2}.variables.C='525'; lib.mat{2}.variables.E='1.15E+11'; lib.mat{2}.variables.nu='0.31'; lib.mat{2}.variables.mu='5E+10'; lib.mat{2}.variables.Sys='9.3E+08'; lib.mat{2}.variables.k='7'; lib.mat{3}.name='Titanium Alloys, General'; lib.mat{3}.variables.alpha='0.0000087'; lib.mat{3}.variables.rho='4700'; lib.mat{3}.variables.sigma='588235.3'; lib.mat{3}.variables.C='525'; lib.mat{3}.variables.E='1.1E+11'; lib.mat{3}.variables.nu='0.33'; lib.mat{3}.variables.mu='4.2E+10'; lib.mat{3}.variables.k='7'; lib.mat{4}.name='Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si), Aged'; lib.mat{4}.variables.alpha='0.000009'; lib.mat{4}.variables.rho='4500'; lib.mat{4}.variables.sigma='625000'; lib.mat{4}.variables.C='525'; lib.mat{4}.variables.E='1.15E+11'; lib.mat{4}.variables.nu='0.31'; lib.mat{4}.variables.mu='5E+10'; lib.mat{4}.variables.Sys='9.4E+08'; lib.mat{4}.variables.k='7';